Customization: | Available |
---|---|
Current: | 2.0 |
Peake Reverse Voltage: | 50-1000 |
Still deciding? Get samples of US$ 0/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
HIGH RELIABILITY-TEST LIST | |||
Number |
Experiment Items |
Experiment Method And Conditions |
Reference |
1 | Solder Resistance |
260ºC+5ºC for 10+2sec. Immerse body into solder 1/16"+1/32" |
MIL-STD-750D METHOD-2031.2 |
2 | Solderability |
230ºC+5ºC for 5 sec. | MIL-STD-750D METHOD-2026.10 |
3 | Pull Test |
1kg in Axial Lead Direction for 10 sec. | MIL-STD-750D METHOD-2036.4 |
4 | Bend Test |
0.5kg Weight Applied To Each Lead Bending Arcs 90 ±5ºC For Three Times |
MIL-STD-750D METHOD-2036.4 |
5 | High Temperature Reverse Bias Test |
TA=100ºC for 1000 Hrs at VR=80% Rated VR | MIL-STD-750D METHOD-1038.4 |
6 | Forward Operation Life Test |
TA=25ºC Rated Average Rectified Current for 500 Hrs |
MIL-STD-750D METHOD-1027.3 |
7 | Intermittent Operation Life |
On state:5 min Tj=125ºC-175ºC with Rated IRMS Power. Off state:5 min Tj=TA+15ºC With Cool Forced Air.On and Off for 1000 Cycles. |
MIL-STD-750D METHOD-1036.3 |
8 | Pressure Cooker |
15 PSIG,TA=121ºC,24hrs | MIL-STD-750D |
9 | Temperature Cycling |
-55ºC/+125ºC 30 Minutes For Dwelled Time 5 Minutes For Transfered Time. Total 10 Cycles. |
MIL-STD-750D METHOD-1051.7 |
10 | Thermal Shock |
0ºC for 5 min,100ºC for 5Min,Total 10 Cycles | MIL-STD-750D METHOD-1056.7 |
11 | Forward Surge |
8.3 ms Single Hale Sine-wave Superimposed On Rated Load, One Surge. |
MIL-STD-750D METHOD-4066.4 |
12 | Humidity Test |
TA=65ºC,RH=98% for 1000hrs. | MIL-STD-750D METHOD-1021.3 |
13 | High Temperature Storage Life |
150ºC for 1000 Hrs | MIL-STD-750D METHOD-1031.5 |